Jinie Technology (Jiangsu) CO ., LTD é um dos fornecedores pioneiros e fabricante do mamilo da liga de monel de qualidade 400, onde fornecemos esses produtos a um preço muito competitivo para os nossos clientes . monet 400 hexagon reduzindo o nppleor é fabricado usando o Optimum Quality StainNeain StainSeny Besides, Monel 400 Hexagon Nipple is made available in various sizes and shapes. Monel 400 One End Threaded Nipple is highly appreciated among our clients for their precise design and durability. As would be expected from its high copper content, Monel 400 Concentric Swaged Nipple is rapidly attacked by nitric acid and ammonia systems. Monel 400 Eccentric Swaged Nipple is a precipitation – hardenable nickel – copper alloy that combines the excellent corrosion resistance characteristic with the added advantage of hardness and greater strength. These amplified properties of strength and hardness in Alloy 400 Hexagon Reducing Nipple is obtained by adding titanium and aluminium to the nickel – copper base and by a thermal processing used to effect precipitation, typically called age endurecimento ou envelhecimento . Nossa liga 400 One End Thread mample pode ser fortalecido pelo trabalho frio antes do endurecimento da precipitação .

 

Especificação do mamilo forjada do Monel 400

Especificações

ASTM B564/ ASME SB564

Especificação de dimensão

ASME 16.11, MSS SP -79, 83, 95, 97, BS 3799

MONEL 400 FORDA FORGENTES

NPT, BSPT, BSPP

MONEL 400 FittingStype

Dn 15- dn1200

Fim

Rosqueado, soldagem, jic

Classificação de pressão de montagem forjada do Monel 400

Extremidade rosqueada -2000 lb/ 3000lb/ 6000lbs acessórios de tubo
End de loda-socket -3000/ 6000/9000 libras

Conexão

Soldagem

Raio de flexão

R =1 d, 2d, 3d, 5d, 6d, 8d, 10d ou acessórios de tubulação personalizados

Faixa de tamanho

½ "NB a 24" NB em sch 10s, 40s, 80s, 160s, xxs . (dn6 ~ dn100)

Processo de fabricação

Empurre, pressione, forja, fundido, etc .

Certificados de teste de acessórios rosqueados do Monel 400

EN 10204/3.1B
Certificado de Matérias -primas
Relatório de teste de radiografia 100%
Relatório de inspeção de terceiros, etc

Mercados e indústrias -chave para acessórios forjados do Monel 400

Atualizadores de betume .

Refinarias de óleo pesado .

Energia nuclear (principalmente sem costura) .

Petroquímicos e ácidos .

Certificados de teste de material (MTC) conforme EN 10204 3.1 e en 10204 3.2, certificados de teste certificando NACE MR0103, NACE MR0175

 

Lista de preços dos mamilos do Monel 400

Alloy 400 mamilo

US $ 0.2-25 / peça (preço do FOB)

MONEL 400 mamilo

US $ 0.2-25 / peça (preço do FOB)

Mamilo de monel

US $ 0.2-25 / peça (preço do FOB)

ASTM B366 MONEL 400 mamilo

US $ 0.2-25 / peça (preço do FOB)

 

Gráfico de tamanho de liga 400 de liga 400 da ASME B16.11

Gráfico de tamanho do mamilo de tubo

Nom . tubo
Tamanho (in)

0.D.

Média
I.D.

Min .
Parede

Nominal
WT ./ft .

Máximo
W . p . psi*

1/8

0.405

0.249

0.068

0.051

810

1/4

0.540

0.344

0.088

0.086

780

3/8

0.675

0.473

0.091

0.115

620

1/2

0.840

0.602

0.109

0.170

600

3/4

1.050

0.804

0.113

0.226

480

1

1.315

1.029

0.133

0.333

450

1-1/4

1.660

1.360

0.140

0.450

370

1-1/2

1.900

1.590

0.145

0.537

330

2

2.375

2.047

0.154

0.720

280

2-1/2

2.875

2.445

0.203

1.136

300

3

3.500

3.042

0.216

1.488

260

3-1/2

4.000

3.521

0.226

1.789

240

4

4.500

3.998

0.237

2.118

220

5

5.563

5.016

0.258

2.874

190

6

6.625

6.031

0.280

3.733

180

8

8.625

7.942

0.322

5.619

160

10

10.750

9.976

0.365

7.966

140

12

12.750

11.889

0.406

10.534

130

14

14.000

13.073

0.437

12.462

130

16

16.000

14.940

0.500

16.286

130

18

18.000

16.809

0.562

20.587

130

20

20.000

18.743

0.593

24.183

120

24

24.000

22.544

0.687

33.652

120

 

Aplicação do mamilo de tubo de monel 400

Os mamilos de tubo de monel 400 são usados ​​em diferentes configurações . aqui é onde você normalmente os encontrará:

Encanamento: a área mais comum onde são encontrados mamilos de tubos de monel 400 é encanamento em um edifício residencial ou comercial . tais mamilos funcionam como conectores para sistemas de tubulação que atendem ao abastecimento de água, remoção de resíduos ou outras funções semelhantes que requerem conexões confiáveis ​​e sem vazamentos .}}}}

Oleodutos industriais: em ambientes industriais, os mamilos de tubo de 400 são usados ​​para conectar a enrolamento industrial de tubulação química, gás ou líquido ., eles são fortes e duráveis, por isso é muito importante nesses locais onde se espera que os acessórios de tubos estejam sob pressão extremamente alta e submetidos a materiais para dar materiais.

 

Caixas elétricas: Monel 400 Mamilos de tubo conectam eletricamente tubos de conduíte a painéis de boxe elétrico em instalação elétrica . Seu objetivo é servir como uma ponte entre o tubo de conduíte elétrico e a caixa .

 

Taincos de cozinha: uma área importante de aplicação está no encanamento da cozinha como parte dos processos estabelecidos para conectar tubos de água aos tubos de torneira da cozinha . O trabalho de um mamilo de tubo de 400 no sistema em sepultamento inclui garantir que os fluxos de água de acordo com faucets ou outros acessórios .}}}}}}} No entanto, os mamilos de tubos Monel 400 podem ser encontrados em algum lugar em quase todos os lugares, os sistemas conectam os tubos . Eles são muito abrangentes e flexíveis e constituem uma boa necessidade na maioria dos setores .

 

Enviar inquérito
Venha até nós
E comece seus RFQs agora.
Contate-nos